Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS2211 BK E70405 - PA610... - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS2211 BK E70405:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid Terra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
High-viscosity, heat- and light-stabilized Polyamide 610 Compound for extrusion
VESTAMID® Terra HS2211 BK E70405 is a polyamide 610 compound developed for the manufacturing of tubing systems with higher demands on heat resistance.

The melting range of VESTAMID® Terra HS2211 BK E70405 is about 40°C higher than PA 11 and PA 12 compounds and allows higher peak temperatures in use.

The compound is especially suitable for the extrusion of tubing systems that are exposed to high burst pressures at high service temperatures, e.g., hydraulic clutch lines. The process temperatures should be within a range of 240°C to 270°C.

VESTAMID® Terra HS2211 is delivered as cylindrical granules ready for processing in moisture-proof packaging. 

VESTAMID® Terra HS is partly based on renewable raw materials and fills the performance gap between the commodity and the niche long-chain nylons.
VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources
.

Pigmentation may affect values.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 19 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
성형 수축률, 평행 1.6 / * % ISO 294-4, 2577
성형 수축률, 수직 1.3 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 2500 / - MPa ISO 527
항복강도 66 / - MPa ISO 527
항복변형률 4 / - % ISO 527
파단시 평균신율 >50 / - % ISO 527
챠피 충격 강도 , +23°C N / - kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C N / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
챠피 노치드 충격 강도, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 222 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 42 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 54 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 155 / * °C ISO 75-1/-2
비카트 연화 온도, B 195 / * °C ISO 306
선형 열팽창 계수, 평행 95 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 94 / * E-6/K ISO 11359-1/-2
기타 특성건조/응축단위시험규격
물에서의 흡수성 3.5 / * % ISO 62와 유사
조건에서의 흡습성 1.7 / * % ISO 62와 유사
밀도 1060 / - kg/m³ ISO 1183
특징
생산 공정
Pipe/Tube Extrusion, 기타 압출
인도 유형
펠렛 (입자,알갱이), 과립, 검정
부가물
이형제
특별 특성
가시광선 안정성, 열안정성
Certifications
Contains renewable resources
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.